SrLaAlO4 (100) ,10x10x0.5mm, 1SP - SLAOa101005S1
Specifications:
- Single crystal SrLaAlO4
- Size: 10mm x 10mm x 0.5mm
- Orientation: (100)
- Orientation tolerance + / - 0.5°
- Surface Roughness <10 Å
- Edge alignment available on request
- Polish: one side EPI polished
Features:
- Good lattice match with perovskite structure superconductors
- Stable structure with much less defects than SrTiO3
- Low dielectric constant suitable for microwave or high frequency application
|
Purity |
99.99% |
|
Color |
Light Brown |
|
Crystal Struture |
Tetragonal |
|
Lattice Constant |
a = b = 3.756 A C = 12.636 A |
|
Density |
5.92 g / cc |
|
Melt Point |
1650 oC |
|
Thermal Expansion Coeff. |
12 ppm / oC |
|
Dielectric Constant |
16.81 at a axis 20.02 at c axis |
Comparison of SrTiO3 - LaAlO3 - SrLaAlO3
|
Properties/Crystal |
SrTiO3 |
LaAlO3 |
SrLaAlO4 |
|
Structure |
Cubic |
Rhombohedral at 25 oC |
Tetragonal |
|
Lattice Constant |
a=3.905 |
a=3.821 A |
a=b=3.756 A c= 12.636 |
|
mismatch to YBCO (a=3.9) |
+0.12% |
-2.0% |
-3.7% |
|
Dielectric Constant |
~300 |
~ 25 |
~ 17 |
|
Grown Method |
Vernuil |
CZ |
CZ |
|
Thermal expansion |
10.4 (x10-6/ oC) |
10 (x10-6/ oC) |
12 (x10-6/ oC) |
|
Melting point |
2080 |
2080 oC |
1650 oC |
|
Density |
5.175 g/cm3 |
6.52 g/cm3 |
5.92 g/cm3 |
|
Max. Crystal Size |
30 mm dia. |
75 mm dia |
35 mm dia |
| Crystal Quality |
Wide rocking curve due to dislocation density |
Visible twin due to phase transition around 400 oC |
Narrow rocking curve, no twins, less defects |
| Crystal Cost |
Higher |
Lower |
Medium |
Related Products
Original: $259.00
-65%$259.00
$90.65SrLaAlO4 (100) ,10x10x0.5mm, 1SP - SLAOa101005S1
Specifications:
- Single crystal SrLaAlO4
- Size: 10mm x 10mm x 0.5mm
- Orientation: (100)
- Orientation tolerance + / - 0.5°
- Surface Roughness <10 Å
- Edge alignment available on request
- Polish: one side EPI polished
Features:
- Good lattice match with perovskite structure superconductors
- Stable structure with much less defects than SrTiO3
- Low dielectric constant suitable for microwave or high frequency application
|
Purity |
99.99% |
|
Color |
Light Brown |
|
Crystal Struture |
Tetragonal |
|
Lattice Constant |
a = b = 3.756 A C = 12.636 A |
|
Density |
5.92 g / cc |
|
Melt Point |
1650 oC |
|
Thermal Expansion Coeff. |
12 ppm / oC |
|
Dielectric Constant |
16.81 at a axis 20.02 at c axis |
Comparison of SrTiO3 - LaAlO3 - SrLaAlO3
|
Properties/Crystal |
SrTiO3 |
LaAlO3 |
SrLaAlO4 |
|
Structure |
Cubic |
Rhombohedral at 25 oC |
Tetragonal |
|
Lattice Constant |
a=3.905 |
a=3.821 A |
a=b=3.756 A c= 12.636 |
|
mismatch to YBCO (a=3.9) |
+0.12% |
-2.0% |
-3.7% |
|
Dielectric Constant |
~300 |
~ 25 |
~ 17 |
|
Grown Method |
Vernuil |
CZ |
CZ |
|
Thermal expansion |
10.4 (x10-6/ oC) |
10 (x10-6/ oC) |
12 (x10-6/ oC) |
|
Melting point |
2080 |
2080 oC |
1650 oC |
|
Density |
5.175 g/cm3 |
6.52 g/cm3 |
5.92 g/cm3 |
|
Max. Crystal Size |
30 mm dia. |
75 mm dia |
35 mm dia |
| Crystal Quality |
Wide rocking curve due to dislocation density |
Visible twin due to phase transition around 400 oC |
Narrow rocking curve, no twins, less defects |
| Crystal Cost |
Higher |
Lower |
Medium |
Related Products
Product Information
Product Information
Shipping & Returns
Shipping & Returns
Description
Specifications:
- Single crystal SrLaAlO4
- Size: 10mm x 10mm x 0.5mm
- Orientation: (100)
- Orientation tolerance + / - 0.5°
- Surface Roughness <10 Å
- Edge alignment available on request
- Polish: one side EPI polished
Features:
- Good lattice match with perovskite structure superconductors
- Stable structure with much less defects than SrTiO3
- Low dielectric constant suitable for microwave or high frequency application
|
Purity |
99.99% |
|
Color |
Light Brown |
|
Crystal Struture |
Tetragonal |
|
Lattice Constant |
a = b = 3.756 A C = 12.636 A |
|
Density |
5.92 g / cc |
|
Melt Point |
1650 oC |
|
Thermal Expansion Coeff. |
12 ppm / oC |
|
Dielectric Constant |
16.81 at a axis 20.02 at c axis |
Comparison of SrTiO3 - LaAlO3 - SrLaAlO3
|
Properties/Crystal |
SrTiO3 |
LaAlO3 |
SrLaAlO4 |
|
Structure |
Cubic |
Rhombohedral at 25 oC |
Tetragonal |
|
Lattice Constant |
a=3.905 |
a=3.821 A |
a=b=3.756 A c= 12.636 |
|
mismatch to YBCO (a=3.9) |
+0.12% |
-2.0% |
-3.7% |
|
Dielectric Constant |
~300 |
~ 25 |
~ 17 |
|
Grown Method |
Vernuil |
CZ |
CZ |
|
Thermal expansion |
10.4 (x10-6/ oC) |
10 (x10-6/ oC) |
12 (x10-6/ oC) |
|
Melting point |
2080 |
2080 oC |
1650 oC |
|
Density |
5.175 g/cm3 |
6.52 g/cm3 |
5.92 g/cm3 |
|
Max. Crystal Size |
30 mm dia. |
75 mm dia |
35 mm dia |
| Crystal Quality |
Wide rocking curve due to dislocation density |
Visible twin due to phase transition around 400 oC |
Narrow rocking curve, no twins, less defects |
| Crystal Cost |
Higher |
Lower |
Medium |