🚚 Free Worldwide Shipping on All Orders!Shop Now
BaTiO3 (001) 10x10x1.0 mm, 2SP, Substrate grade (with domains)
HomeStore

BaTiO3 (001) 10x10x1.0 mm, 2SP, Substrate grade (with domains)

BaTiO3 (001) 10x10x1.0 mm, 2SP, Substrate grade (with domains)

Substrate Specifications

  • Crystal Grade:         Single Crystal with substrate grade (with domains) 
  • Size:                       10 x10 x 1.0 mm +/- 0.05 mm
  • Polished:                 two sides   polished 
  •  Orientation:              <001> +/- 0.5 o
  • Packing:                   1000 class clean room in vacuum bag
  • Shipping:                  in a thermal box with battery pack to keep substrate > 13oC

    Typical  Properties of BaTiO3 single crystal

    Crystal Structure

    • Tetragonal ( 4m) : 9oC < T < 130.5 oC
    • a=3.99  A  c= 4.04 A

    Growth Method

    Top Seeded Solution Growth

    Melting Point

    1600 oC

    Density

     6.02  g/cm3

    Dielectric constants

    • ea = 3700, ec = 135 (unclamped)
    • ea = 2400, e c = 60 (clamped)

    Index of Refraction

     

    •                 515 nm               633 nm     800 nm
    • no            2.4921                   2.4160                   2.3681
    • ne            2.4247                   2.3630                   2.3235

    Transmission wavelength

    0.45 ~ 6.30 mm

    Electro Optic Coefficients:

    rT 13 =      11.7 ?1.9 pm/V     rT 33 =112 ?10  pm/V    rT 42=       1920 ?180  pm/V

    Reflectivity of SPPC
    ( at 0 deg. cut )

    • 50 - 70 % ( max. 77% ) for l = 515 nm
    • 50 - 80 % ( max: 86.8%) for l = 633 nm
    Two-wave mixing coupling constant: 10 -40  cm-1

    Absorption loss: 

    • l:             515 nm               633 nm                   800 nm
    • a:            3.392cm-1              0.268cm-1              0.005cm-1

    Related Product

    Other Crystal wafer A-Z

    Plasma Cleaner

     Wafer Containers

    Dicing saw

    Film Coater

     
$384.65

Original: $1,099.00

-65%
BaTiO3 (001) 10x10x1.0 mm, 2SP, Substrate grade (with domains)

$1,099.00

$384.65

BaTiO3 (001) 10x10x1.0 mm, 2SP, Substrate grade (with domains)

Substrate Specifications

  • Crystal Grade:         Single Crystal with substrate grade (with domains) 
  • Size:                       10 x10 x 1.0 mm +/- 0.05 mm
  • Polished:                 two sides   polished 
  •  Orientation:              <001> +/- 0.5 o
  • Packing:                   1000 class clean room in vacuum bag
  • Shipping:                  in a thermal box with battery pack to keep substrate > 13oC

    Typical  Properties of BaTiO3 single crystal

    Crystal Structure

    • Tetragonal ( 4m) : 9oC < T < 130.5 oC
    • a=3.99  A  c= 4.04 A

    Growth Method

    Top Seeded Solution Growth

    Melting Point

    1600 oC

    Density

     6.02  g/cm3

    Dielectric constants

    • ea = 3700, ec = 135 (unclamped)
    • ea = 2400, e c = 60 (clamped)

    Index of Refraction

     

    •                 515 nm               633 nm     800 nm
    • no            2.4921                   2.4160                   2.3681
    • ne            2.4247                   2.3630                   2.3235

    Transmission wavelength

    0.45 ~ 6.30 mm

    Electro Optic Coefficients:

    rT 13 =      11.7 ?1.9 pm/V     rT 33 =112 ?10  pm/V    rT 42=       1920 ?180  pm/V

    Reflectivity of SPPC
    ( at 0 deg. cut )

    • 50 - 70 % ( max. 77% ) for l = 515 nm
    • 50 - 80 % ( max: 86.8%) for l = 633 nm
    Two-wave mixing coupling constant: 10 -40  cm-1

    Absorption loss: 

    • l:             515 nm               633 nm                   800 nm
    • a:            3.392cm-1              0.268cm-1              0.005cm-1

    Related Product

    Other Crystal wafer A-Z

    Plasma Cleaner

     Wafer Containers

    Dicing saw

    Film Coater

     

Product Information

Shipping & Returns

Description

Substrate Specifications

  • Crystal Grade:         Single Crystal with substrate grade (with domains) 
  • Size:                       10 x10 x 1.0 mm +/- 0.05 mm
  • Polished:                 two sides   polished 
  •  Orientation:              <001> +/- 0.5 o
  • Packing:                   1000 class clean room in vacuum bag
  • Shipping:                  in a thermal box with battery pack to keep substrate > 13oC

    Typical  Properties of BaTiO3 single crystal

    Crystal Structure

    • Tetragonal ( 4m) : 9oC < T < 130.5 oC
    • a=3.99  A  c= 4.04 A

    Growth Method

    Top Seeded Solution Growth

    Melting Point

    1600 oC

    Density

     6.02  g/cm3

    Dielectric constants

    • ea = 3700, ec = 135 (unclamped)
    • ea = 2400, e c = 60 (clamped)

    Index of Refraction

     

    •                 515 nm               633 nm     800 nm
    • no            2.4921                   2.4160                   2.3681
    • ne            2.4247                   2.3630                   2.3235

    Transmission wavelength

    0.45 ~ 6.30 mm

    Electro Optic Coefficients:

    rT 13 =      11.7 ?1.9 pm/V     rT 33 =112 ?10  pm/V    rT 42=       1920 ?180  pm/V

    Reflectivity of SPPC
    ( at 0 deg. cut )

    • 50 - 70 % ( max. 77% ) for l = 515 nm
    • 50 - 80 % ( max: 86.8%) for l = 633 nm
    Two-wave mixing coupling constant: 10 -40  cm-1

    Absorption loss: 

    • l:             515 nm               633 nm                   800 nm
    • a:            3.392cm-1              0.268cm-1              0.005cm-1

    Related Product

    Other Crystal wafer A-Z

    Plasma Cleaner

     Wafer Containers

    Dicing saw

    Film Coater

     