🚚 Free Worldwide Shipping on All Orders!Shop Now
BaTiO3 (001) 5x5x1.0 mm, 1SP, Substrate grade with single domain
HomeStore

BaTiO3 (001) 5x5x1.0 mm, 1SP, Substrate grade with single domain

BaTiO3 (001) 5x5x1.0 mm, 1SP, Substrate grade with single domain

Substrate Specifications

  • Crystal Grade:         Single Crystal with  substrate grade with single domain 
  • Size:                       5 x5 x 1.0 mm +/- 0.05 mm
  • Polished:                 One side  polished 
  •  Orientation:              <001> +/- 0.5 o
  • Packing:                   1000 class clean room in vacuum bag
  • Shipping:                  in a thermal box with battery pack to keep substrate > 13o
     

 

Typical  Properties of BaTiO3 single crystal

Crystal Structure

  • Tetragonal ( 4m) : 9oC < T < 130.5 oC
  • a=3.99  A  c= 4.04 A

Growth Method

Top Seeded Solution Growth

Melting Point

1600 oC

Density

 6.02  g/cm3

Dielectric constants

  • ea = 3700, ec = 135 (unclamped)
  • ea = 2400, e c = 60 (clamped)

Index of Refraction

 

  •                 515 nm               633 nm     800 nm
  • no            2.4921                   2.4160                   2.3681
  • ne            2.4247                   2.3630                   2.3235

Transmission wavelength

0.45 ~ 6.30 mm

Electro Optic Coefficients:

rT 13 =      11.7 ?1.9 pm/V     rT 33 =112 ?10  pm/V    rT 42=       1920 ?180  pm/V

Reflectivity of SPPC
( at 0 deg. cut )

  • 50 - 70 % ( max. 77% ) for l = 515 nm
  • 50 - 80 % ( max: 86.8%) for l = 633 nm
Two-wave mixing coupling constant: 10 -40  cm-1

Absorption loss: 

  • l:             515 nm               633 nm                   800 nm
  • a:            3.392cm-1              0.268cm-1              0.005cm-1

Related Product

Other Crystal wafer A-Z

Plasma Cleaner

 Wafer Containers

Dicing saw

Film Coater

$659.00
BaTiO3 (001) 5x5x1.0 mm, 1SP, Substrate grade with single domain
$659.00

BaTiO3 (001) 5x5x1.0 mm, 1SP, Substrate grade with single domain

Substrate Specifications

  • Crystal Grade:         Single Crystal with  substrate grade with single domain 
  • Size:                       5 x5 x 1.0 mm +/- 0.05 mm
  • Polished:                 One side  polished 
  •  Orientation:              <001> +/- 0.5 o
  • Packing:                   1000 class clean room in vacuum bag
  • Shipping:                  in a thermal box with battery pack to keep substrate > 13o
     

 

Typical  Properties of BaTiO3 single crystal

Crystal Structure

  • Tetragonal ( 4m) : 9oC < T < 130.5 oC
  • a=3.99  A  c= 4.04 A

Growth Method

Top Seeded Solution Growth

Melting Point

1600 oC

Density

 6.02  g/cm3

Dielectric constants

  • ea = 3700, ec = 135 (unclamped)
  • ea = 2400, e c = 60 (clamped)

Index of Refraction

 

  •                 515 nm               633 nm     800 nm
  • no            2.4921                   2.4160                   2.3681
  • ne            2.4247                   2.3630                   2.3235

Transmission wavelength

0.45 ~ 6.30 mm

Electro Optic Coefficients:

rT 13 =      11.7 ?1.9 pm/V     rT 33 =112 ?10  pm/V    rT 42=       1920 ?180  pm/V

Reflectivity of SPPC
( at 0 deg. cut )

  • 50 - 70 % ( max. 77% ) for l = 515 nm
  • 50 - 80 % ( max: 86.8%) for l = 633 nm
Two-wave mixing coupling constant: 10 -40  cm-1

Absorption loss: 

  • l:             515 nm               633 nm                   800 nm
  • a:            3.392cm-1              0.268cm-1              0.005cm-1

Related Product

Other Crystal wafer A-Z

Plasma Cleaner

 Wafer Containers

Dicing saw

Film Coater

Product Information

Shipping & Returns

Description

Substrate Specifications

  • Crystal Grade:         Single Crystal with  substrate grade with single domain 
  • Size:                       5 x5 x 1.0 mm +/- 0.05 mm
  • Polished:                 One side  polished 
  •  Orientation:              <001> +/- 0.5 o
  • Packing:                   1000 class clean room in vacuum bag
  • Shipping:                  in a thermal box with battery pack to keep substrate > 13o
     

 

Typical  Properties of BaTiO3 single crystal

Crystal Structure

  • Tetragonal ( 4m) : 9oC < T < 130.5 oC
  • a=3.99  A  c= 4.04 A

Growth Method

Top Seeded Solution Growth

Melting Point

1600 oC

Density

 6.02  g/cm3

Dielectric constants

  • ea = 3700, ec = 135 (unclamped)
  • ea = 2400, e c = 60 (clamped)

Index of Refraction

 

  •                 515 nm               633 nm     800 nm
  • no            2.4921                   2.4160                   2.3681
  • ne            2.4247                   2.3630                   2.3235

Transmission wavelength

0.45 ~ 6.30 mm

Electro Optic Coefficients:

rT 13 =      11.7 ?1.9 pm/V     rT 33 =112 ?10  pm/V    rT 42=       1920 ?180  pm/V

Reflectivity of SPPC
( at 0 deg. cut )

  • 50 - 70 % ( max. 77% ) for l = 515 nm
  • 50 - 80 % ( max: 86.8%) for l = 633 nm
Two-wave mixing coupling constant: 10 -40  cm-1

Absorption loss: 

  • l:             515 nm               633 nm                   800 nm
  • a:            3.392cm-1              0.268cm-1              0.005cm-1