Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with Alumina Coating for Li-ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCA
HomeStore

Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with Alumina Coating for Li-ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCA

Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with Alumina Coating for Li-ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCA

Single Crystal powder of LiNiCoMnO2 (Lithium Nickel Manganese Cobalt Oxide, Ni:Co:Mn=8:1:1, NCM811 or NMC811) with Alumina coating is a excellent cathode powder with high stability for solid-state lithium-ion battery application.Ā 


Specification

Properties Item Typical Value

Chemical Composition
Ni (mol%) 82.1%
Co (mol%) 12.0%
Mn (mol%) 5.9%


Particle Size Distribution

D10 (μm)  2.1
D50 (μm) 4.5
D90 (μm) 8.3
Specific Surface Area (m2/g) BET 0.95
Tap Density (g/cm³)
1.58

Ā 
Specific Capacity (mAh/g)Ā 

0.1 C 201 mAh/g

Columbic Efficiency (first cycle)

0.1C 88.5%

Note
MTI does not manufacture this product,Ā and only sell the small quantity to research for development for new generationĀ battery. If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer.



Application Notes
:

  1. Please click to see Procedure forĀ Preparing Anode & Cathode Electrode Slurry.
  2. Please keep the powder in the vacuum box to avoid moisture.
  3. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
  4. The productĀ is for research only,Ā not supply for large quantity,Ā 

Ā 

$298.00
Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with Alumina Coating for Li-ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCA—
$298.00

Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with Alumina Coating for Li-ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCA

Single Crystal powder of LiNiCoMnO2 (Lithium Nickel Manganese Cobalt Oxide, Ni:Co:Mn=8:1:1, NCM811 or NMC811) with Alumina coating is a excellent cathode powder with high stability for solid-state lithium-ion battery application.Ā 


Specification

Properties Item Typical Value

Chemical Composition
Ni (mol%) 82.1%
Co (mol%) 12.0%
Mn (mol%) 5.9%


Particle Size Distribution

D10 (μm)  2.1
D50 (μm) 4.5
D90 (μm) 8.3
Specific Surface Area (m2/g) BET 0.95
Tap Density (g/cm³)
1.58

Ā 
Specific Capacity (mAh/g)Ā 

0.1 C 201 mAh/g

Columbic Efficiency (first cycle)

0.1C 88.5%

Note
MTI does not manufacture this product,Ā and only sell the small quantity to research for development for new generationĀ battery. If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer.



Application Notes
:

  1. Please click to see Procedure forĀ Preparing Anode & Cathode Electrode Slurry.
  2. Please keep the powder in the vacuum box to avoid moisture.
  3. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
  4. The productĀ is for research only,Ā not supply for large quantity,Ā 

Ā 

Product Information

Shipping & Returns

Description

Single Crystal powder of LiNiCoMnO2 (Lithium Nickel Manganese Cobalt Oxide, Ni:Co:Mn=8:1:1, NCM811 or NMC811) with Alumina coating is a excellent cathode powder with high stability for solid-state lithium-ion battery application.Ā 


Specification

Properties Item Typical Value

Chemical Composition
Ni (mol%) 82.1%
Co (mol%) 12.0%
Mn (mol%) 5.9%


Particle Size Distribution

D10 (μm)  2.1
D50 (μm) 4.5
D90 (μm) 8.3
Specific Surface Area (m2/g) BET 0.95
Tap Density (g/cm³)
1.58

Ā 
Specific Capacity (mAh/g)Ā 

0.1 C 201 mAh/g

Columbic Efficiency (first cycle)

0.1C 88.5%

Note
MTI does not manufacture this product,Ā and only sell the small quantity to research for development for new generationĀ battery. If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer.



Application Notes
:

  1. Please click to see Procedure forĀ Preparing Anode & Cathode Electrode Slurry.
  2. Please keep the powder in the vacuum box to avoid moisture.
  3. Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
  4. The productĀ is for research only,Ā not supply for large quantity,Ā 

Ā 

Single Crystal Powder of LiNiCoMnO2 (Ni:Co:Mn=8:1:1, NCM811) with Alumina Coating for Li-ion Battery Cathode, 200g/bottle - Lib-LNCM811-SCA | MTI Online Store