NASICON-Type LATP (Li1.3AI0.3Ti1.7P3O12) Powder as Solid-State Electrolyte for Li-ion Battery, 100g/bottle-Lib-LATP
NASICON-Type LATP (Li1.3AI0.3Ti1.7P3O12) Powder as Solid-State Electrolyte for Li-ion Battery, 100g/bottle-Lib-LATP
NASICON-Type LATP (Li.3AI0.3Ti1.7P3O12) powder as solid-state electrolyte for Li-on battery research & education, 100g/bottle-Lib-LATP
Specification
| Product Name |
|
| Chemical Formula |
|
| Main Crystalline Phase |
|
| Appearance |
|
| Powder Size |
|
| Ionic Conductivity |
|
| Water Level |
|
| pH |
|
| SEM | |
| XRD | |
| Impedance Spectrum |
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in the vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 -150 °C before making slurry and coating to ensure max. capacity.
- The product is for research only, not supply for large quantity.
Original: $498.00
-65%$498.00
$174.30More Images

NASICON-Type LATP (Li1.3AI0.3Ti1.7P3O12) Powder as Solid-State Electrolyte for Li-ion Battery, 100g/bottle-Lib-LATP
NASICON-Type LATP (Li.3AI0.3Ti1.7P3O12) powder as solid-state electrolyte for Li-on battery research & education, 100g/bottle-Lib-LATP
Specification
| Product Name |
|
| Chemical Formula |
|
| Main Crystalline Phase |
|
| Appearance |
|
| Powder Size |
|
| Ionic Conductivity |
|
| Water Level |
|
| pH |
|
| SEM | |
| XRD | |
| Impedance Spectrum |
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in the vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 -150 °C before making slurry and coating to ensure max. capacity.
- The product is for research only, not supply for large quantity.
Product Information
Product Information
Shipping & Returns
Shipping & Returns
Description
NASICON-Type LATP (Li.3AI0.3Ti1.7P3O12) powder as solid-state electrolyte for Li-on battery research & education, 100g/bottle-Lib-LATP
Specification
| Product Name |
|
| Chemical Formula |
|
| Main Crystalline Phase |
|
| Appearance |
|
| Powder Size |
|
| Ionic Conductivity |
|
| Water Level |
|
| pH |
|
| SEM | |
| XRD | |
| Impedance Spectrum |
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in the vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 -150 °C before making slurry and coating to ensure max. capacity.
- The product is for research only, not supply for large quantity.