🚚 Free Worldwide Shipping on All Orders!Shop Now
DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF
HomeStore

DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF

DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF

The DNP aluminum laminated filmĀ (91 um) is used as a casing materialĀ for the polymerĀ Li-Ion battery, which is made in Japan

Specifications

Layers by Layer

  • Matte Ink Layer: 3.0 g /m^2 ± 0.5 g/m^2
  • Biaxially Oriented Nylon (ONy); 6-Nylon: 15 um ± 10%
  • Adhesive Layer (Carbon Black Mixed): 3.8 g/m^2 ± 1.5 g/m^2
  • Mat Surface (Treatment Layer)
  • Soft Aluminum Foil (ALM): 8021 or 8079; 35Ā  um ± 10%
    Glossy Surface (Treatment Layer)
    Adhesive Resin Layer (PPa): Acid-modified PP;20 um ± 10%
    Polypropylene (PP): 15 um ± 10%
  • Glossy Surface (Treatment Layer)
  • Adhesive Resin Layer (PPa): Acid-modified PP;20 um ± 10%
  • Polypropylene (PP): 15 um ± 10%
ThicknessĀ  Ā  Ā  Ā 
  • 91 μm ± 10%Ā 
Width and Length
  • DNP-ALF30: Width 120 mm  ± 0.5 mm x Length 30m
  • DNP-ALF50:Ā  Width 400 mm ± 0.5 mm x Length 50m
  • DNP-ALF300: Width 400 mm ± 0.5 mm x LengthĀ  300m
Heat Seal Strength
  • 30 N / 15 mm or more
Laminate Strength ONy / ALM
  • 3.0 N / 15 mm or more
Laminate Strength ALM / PP
  • 5.0 N / 15 mm or more
Electrolyte Resistance ALM / PP
  • 4.0 N / 15 mm or more
  • Dip Brazing 85°C, 24 hours
Surface quality
  • Mat finish
Fish Eye
  • 2mm or less in diameter (clear)
  • 1mm or less in diameter (colored)
Molding Depth
  • < 8.0mm
Electrical Insulating
  • Good
Hot Sealing Condition
  • 180-190°C
Moisture Vapor / O2 Transmission Rate
  • 200ppm / 5 yearsĀ 
Solvent Retention
  • Less than 5mg/m2
Appearance
  • Within the sample of the limit
Slip Factor
  • CPP/CPPĀ Ā  less than 1.0
SDS
Application Notes & Video

  • Click the picture below to see the finished polymer Li-Ion battery made by the heated sealer
    Ā 

Ā 

Ā 

Ā 

Select Length
From $439.00
DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF—
$439.00

More Images

DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF - Image 2
DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF - Image 3

DNP Aluminum Laminated Film for Pouch Cell Case - DNP-ALF

The DNP aluminum laminated filmĀ (91 um) is used as a casing materialĀ for the polymerĀ Li-Ion battery, which is made in Japan

Specifications

Layers by Layer

  • Matte Ink Layer: 3.0 g /m^2 ± 0.5 g/m^2
  • Biaxially Oriented Nylon (ONy); 6-Nylon: 15 um ± 10%
  • Adhesive Layer (Carbon Black Mixed): 3.8 g/m^2 ± 1.5 g/m^2
  • Mat Surface (Treatment Layer)
  • Soft Aluminum Foil (ALM): 8021 or 8079; 35Ā  um ± 10%
    Glossy Surface (Treatment Layer)
    Adhesive Resin Layer (PPa): Acid-modified PP;20 um ± 10%
    Polypropylene (PP): 15 um ± 10%
  • Glossy Surface (Treatment Layer)
  • Adhesive Resin Layer (PPa): Acid-modified PP;20 um ± 10%
  • Polypropylene (PP): 15 um ± 10%
ThicknessĀ  Ā  Ā  Ā 
  • 91 μm ± 10%Ā 
Width and Length
  • DNP-ALF30: Width 120 mm  ± 0.5 mm x Length 30m
  • DNP-ALF50:Ā  Width 400 mm ± 0.5 mm x Length 50m
  • DNP-ALF300: Width 400 mm ± 0.5 mm x LengthĀ  300m
Heat Seal Strength
  • 30 N / 15 mm or more
Laminate Strength ONy / ALM
  • 3.0 N / 15 mm or more
Laminate Strength ALM / PP
  • 5.0 N / 15 mm or more
Electrolyte Resistance ALM / PP
  • 4.0 N / 15 mm or more
  • Dip Brazing 85°C, 24 hours
Surface quality
  • Mat finish
Fish Eye
  • 2mm or less in diameter (clear)
  • 1mm or less in diameter (colored)
Molding Depth
  • < 8.0mm
Electrical Insulating
  • Good
Hot Sealing Condition
  • 180-190°C
Moisture Vapor / O2 Transmission Rate
  • 200ppm / 5 yearsĀ 
Solvent Retention
  • Less than 5mg/m2
Appearance
  • Within the sample of the limit
Slip Factor
  • CPP/CPPĀ Ā  less than 1.0
SDS
Application Notes & Video

  • Click the picture below to see the finished polymer Li-Ion battery made by the heated sealer
    Ā 

Ā 

Ā 

Ā 

Product Information

Shipping & Returns

Description

The DNP aluminum laminated filmĀ (91 um) is used as a casing materialĀ for the polymerĀ Li-Ion battery, which is made in Japan

Specifications

Layers by Layer

  • Matte Ink Layer: 3.0 g /m^2 ± 0.5 g/m^2
  • Biaxially Oriented Nylon (ONy); 6-Nylon: 15 um ± 10%
  • Adhesive Layer (Carbon Black Mixed): 3.8 g/m^2 ± 1.5 g/m^2
  • Mat Surface (Treatment Layer)
  • Soft Aluminum Foil (ALM): 8021 or 8079; 35Ā  um ± 10%
    Glossy Surface (Treatment Layer)
    Adhesive Resin Layer (PPa): Acid-modified PP;20 um ± 10%
    Polypropylene (PP): 15 um ± 10%
  • Glossy Surface (Treatment Layer)
  • Adhesive Resin Layer (PPa): Acid-modified PP;20 um ± 10%
  • Polypropylene (PP): 15 um ± 10%
ThicknessĀ  Ā  Ā  Ā 
  • 91 μm ± 10%Ā 
Width and Length
  • DNP-ALF30: Width 120 mm  ± 0.5 mm x Length 30m
  • DNP-ALF50:Ā  Width 400 mm ± 0.5 mm x Length 50m
  • DNP-ALF300: Width 400 mm ± 0.5 mm x LengthĀ  300m
Heat Seal Strength
  • 30 N / 15 mm or more
Laminate Strength ONy / ALM
  • 3.0 N / 15 mm or more
Laminate Strength ALM / PP
  • 5.0 N / 15 mm or more
Electrolyte Resistance ALM / PP
  • 4.0 N / 15 mm or more
  • Dip Brazing 85°C, 24 hours
Surface quality
  • Mat finish
Fish Eye
  • 2mm or less in diameter (clear)
  • 1mm or less in diameter (colored)
Molding Depth
  • < 8.0mm
Electrical Insulating
  • Good
Hot Sealing Condition
  • 180-190°C
Moisture Vapor / O2 Transmission Rate
  • 200ppm / 5 yearsĀ 
Solvent Retention
  • Less than 5mg/m2
Appearance
  • Within the sample of the limit
Slip Factor
  • CPP/CPPĀ Ā  less than 1.0
SDS
Application Notes & Video

  • Click the picture below to see the finished polymer Li-Ion battery made by the heated sealer
    Ā 

Ā 

Ā 

Ā